- Bore Diameter
- 0.5620 inches minimum and 0.5625 inches maximum
- Hardness Rating
- 55.0 rockwell c minimum and 62.0 rockwell c maximum inner member
- Hardness Rating
- 28.0 rockwell c minimum and 37.0 rockwell c maximum outer race member
- Inner Member Width
- 0.685 inches minimum and 0.687 inches maximum
- Lubrication Feature
- self-lubricating liner race liner
- Part Name Assigned By Controlling Agency
- bearing, plain, self-lubricating, self-aligning, low speed, wide, grooved race, -65 to +325 f
- Material Document And Classification
- ams5630 international std/spec all material responses or ams5880 international std/spec all material responses or ams5618 international std/spec all material responses inner member
- Material Document And Classification
- ams5643 international std/spec all material responses outer race member
- Material
- plastic polytetrafluoroethylene race liner
- Material
- steel comp 440c inner member
- Material
- steel corrosion resisting outer race member
- Outer Member Outside Diameter
- 1.1245 inches minimum and 1.1250 inches maximum
- Outer Member Width
- 0.531 inches minimum and 0.541 inches maximum
- Special Features
- absence of letter c indicates 440c ball material. letter a = tested to 100,000 cycles. p = zinc-nickel or cadmium plating. material - ball: 440c (ams5630, ams5880, or ams5618). race: 17-4ph cres per ams5643. liner: ptfe shall be included in the liner. harness rating is before swaging. finish: race: plating, when specified, shall be zinc-nickel plating per ams2417, type 2, grade b or cadmium plating per ams-qq-p-416, type ii, class 2. plating shall be on the outside diameter surface and on the flats between the outside diameter and the v-grooves. the plating runout shall occur either in the v-grooves or on the side face areas between the v-grooves and the ball. ball: passivate per ams2700, method 1 (nitric acid) or method 2 (citric acid), or astm a967. citric 1, citric 2, and citric 3 are acceptable. (ams2700, method 1, type 8 is prohibited on bearings manufactured with 440c after june 1, 2018).
- Static Radial Load Rating
- 26600 pounds
- Style Designator
- with insert and/or liner with staking groove
- Surface Treatment Document And Classification
- ams2417, type 2, grade b international std/spec all treatment responses or ams-qq-p-416, type ii, class 2 international std/spec all treatment responses inner member
- Surface Treatment Document And Classification
- ams2700, method 1 (nitric acid) or method 2 (citric acid) international std/spec all treatment responses or astm a967. citric 1, citric 2, and citric 3 international std/spec all treatment responses outer race member
- Surface Treatment
- cadmium or zinc and nickel alloy inner member
- Surface Treatment
- passivate outer race member